Coils of bright rolled steel strip stood on end in a hall
How the joint works

The fold does the holding

Solder is soft. You can mark it with a thumbnail. Nothing that has to carry fourteen litres up a ladder is held together by it, and any seam that looks like a bead of metal laid along a gap will open the first time the piece is dropped.

From flat sheet to a locked edge

One

Cut, with the allowance on

The blank is marked three times the metal thickness wider than the finished body on each joining edge. Forget the allowance and the piece comes out short, and there is no adding it back.

Two

Fold both edges into hooks

Each edge goes over a bar and comes back on itself. Hooked together and run down with a groover, the two hooks pull against one another. That alone will hold the body closed, dry.

Three

Flux it and let it draw

Clean metal, zinc-chloride flux, a hot tinned bit held long enough for the sheet itself to take the heat. The solder is pulled into the fold by the gap, not pushed in. Wipe, and almost nothing shows.

A sheet of corrugated grey metal

Why a wire goes into a rim

A rim is the weakest line on a pail. Grab a full one by a raw folded edge and the circle goes oval, and once it is oval the lid never sits again. So the top 12 mm is rolled around a 2.5 mm soft wire and closed. The wire is doing the work; the tin is only wrapped round it. You can feel it through the fold.

Rim wire is on the Tools shelf at €18 for ten metres.

A hammered metal pot catching a shaft of light on a dark bench

The hammer stiffens the panel

Thin sheet drums and dents. Planishing it over a stake with a flat-faced hammer spreads the metal a fraction and leaves a field of shallow overlapping marks that will not come out. The panel goes hard, it stops ringing, and the light finally sits on it instead of sliding off.

Every pail body is planished before the bottom goes in.

What people ask about solder

Could you not just run solder down the gap?

You can, and it holds for a season. A fillet laid over a butt joint puts the whole load on a metal that bends under a thumbnail, so it cracks as soon as the body flexes. A fold takes the load; the solder only has to keep the milk on the inside.

Why has my old pail gone rusty in one spot only?

Something cut through the tin there. Tinplate is steel with a coat of tin on it, and the coat is thinner than paper. Scratch it and the steel underneath is open to the air, so the rust starts at the scratch and creeps out from it while the rest of the pail stays bright.

Which bar is in which seam?

Dairy ware and the skimmer get a lead-free tin-silver bar, kept on its own shelf with its own iron so nothing crosses over. Lanterns, the watering can and stove pipe get 40/60 tin-lead. Each piece leaves with a note saying which. We hold no food-contact certificate and will not pretend otherwise.

Can a grooved seam be opened again?

Yes, and that is exactly what it is for. Heat the seam until the solder lets go, unhook the fold, and the two edges come apart with the metal intact. That is how a bottom comes out of a body for re-tinning and goes back in afterwards.

Sixteen pieces, all folded this way

Pails, cans, lanterns, pipe and the tools to keep them going, on one page with the prices beside them.